Publication: Use of polyamides that are resistant to corrosion and stress cracking
Loading...
Date
2014
Journal Title
Journal ISSN
Volume Title
Publisher
Abstract
The use of thermoplastic molding materials comprising A) 10 to 98.8% by weight of a mixture formed from a1) 40 to 70% by weight of nylon-6,6 or nylon-4,6 or nylon-6 or mixtures thereof, a2) 30 to 60% by weight of a polyamide having a ratio of methylene to amide groups of 7 to 12, B) 1 to 50% by weight of a fibrous or particulate filler, C) 0.1 to 3% by weight of a lubricant, D) 0.05 to 3% by weight of a heat stabilizer, E) 0 to 40% by weight of further additives, where the sum of the percentages by weight A) to E) and a1) and a2) adds to 100%, for production of stress cracking- and corrosion-resistant moldings.